What is the cause of bubbles in the production of PET Bottles?

What is the cause of bubbles in the production of PET Bottles?

Update:23 Jun 2022

PET Bottles is a kind of plastic container, which uses PET, PE and PP as raw materials, adds the corresponding organic solvent, heats it at high temperature, and then blows, extrudes or even injection-molded. Sprayer Bottles are not easy to break, low cost, high transparency, food grade materials, etc. Data Side Effects It is said that long-term consumption of foods contaminated with polyethylene molecules can cause dizziness, headache, bad appetite, loss of appetite, and memory loss. even anemia. Therefore, packaging vinegar in plastic bottles is harmful to human health. Therefore, glassware should be eaten at home instead of plastic products to hold seasonings. Take special care when working with plastics and do not touch vinegar, detergents, etc. Avoid direct sunlight, high temperature, etc. and prevent chemical reactions. In addition, when purchasing plastic tableware, you should choose plastic products with PE (polyethylene) or PP (polypropylene) logo, few decorative pictures, colorless and odorless, and smooth surface.
1. Material factors 1. Raw materials contain moisture 2. Mold factors 3. The mold is trapped in the air, so the mold should be maintained or an exhaust slot should be added. Therefore, we must pay attention to these aspects in the summary of the production process.
1. Material factors
1. Raw materials contain moisture
2. Mold factor
3. The mold is trapped in the air, so the mold should be maintained or an exhaust slot should be added
Therefore, we must pay attention to these aspects in the production process in order to make beautiful bottles.
2. Technical factors
1. The speed is too fast, so that the molten plastic is decomposed under the action of large shear, and gas is generated.
2. The local cooling of the product is too fast and the shrinkage is uneven. Especially when the wall thickness of the product is large, the surface cooling rate is faster than that of the central part. During the cooling process, the plastic in the center part shrinks and expands outward, making the center part insufficiently filled and forming a vacuum bubble.
3. Insufficient pressure and holding pressure make the melt not close to the surface of the cavity, which is not conducive to exhausting.
4. Insufficient back pressure, control the backward speed of the screw rod. When the back pressure is small, the screw retreats faster, which easily leads to insufficient feed. There is a lot of air brought into the material, and it is too late to be discharged from the feed port, resulting in a large number of air bubbles.

0

Ningbo Jazz Packaging Co.,Ltd.

  • Disposable clear PET plastic sprayer bottler

    Disposable clear PET plastic sprayer bottler

  • High level round airless bottle white airless bottle 5ml 10ml 15ml airless bottle

    High level round airless bottle white airless bottle 5ml 10ml 15ml airless bottle

  • 1.20-1.50ml/T 28/410 left right lotion pump

    1.20-1.50ml/T 28/410 left right lotion pump

  • plastic deodorant roller ball bottle

    plastic deodorant roller ball bottle

  • Roll on bottle & Deodorant Stick JZ6517

    Roll on bottle & Deodorant Stick JZ6517

  • Cream Jar JZ514

    Cream Jar JZ514

  • 250ML 450ML 650ML Plastic Square Bottle For Lotion Soap Pump

    250ML 450ML 650ML Plastic Square Bottle For Lotion Soap Pump

  • roll on bottle with roller ball

    roll on bottle with roller ball